Spherulite growth of L-lactide copolymers: Effects of tacticity and comonomers

Journal

POLYMER
Volume 46, Issue 13, Pages 4917-4927

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/j.polymer.2005.03.069

Keywords

poly(L-lactide); L-lactide copolymers; spherulite growth

Ask authors/readers for more resources

The spherulite growth behavior and mechanism of L-lactide copolymers, poly (L-lactide-co-D-lactide) [P(LLA-DLA)], poly(L-lactide-co-glycolide) [P(LLA-GA)], and poly(L-lactide-co-epsilon-caprolactone) [P(LLA-CL)] have been studied using polarization optical microscopy in comparison with poly(L-lactide) (PLLA) having different molecular weights to elucidate the effects of incorporated comonomer units. The incorporation of comonomer units reduced the radius growth rate of spherulites (G) and increased the induction period of spherulite formation (t(i)), irrespective of the kind of comonomer unit. Such effects became remarkable with the content of comonomers. At a crystallization temperature (T-c) of 130 degrees C, the disturbance effects of comonomers on the spherulite growth decreased in the following order: D-lactide > glycolide > epsilon-caprolactone, when compared at the same comonomer unit or reciprocal of averaged L-lactyl unit sequence length (l(L)). The t(i) estimation indicated that the glycolide units have the lowest disturbance effects on the formation of spherulite (crystallite) nuclei. The PLLA having the number-average molecular weight (M-n) exceeding 3.1 X 10(4) g mol(-1) showed the transition from regime II to regime III at T-c = 120 degrees C, whereas PLLA with the lowest M-n of 9.2 X 10(3) g mol(-1) crystallized solely in regime III kinetics and the copolymers excluding P(LLA-DLA) with 3% of D-lactide units crystallized solely according to regime II kinetics. The nucleation and front constant for regime II and III [K-g(II), K-g(III), G(0)(II), and G(0)(III), respectively] estimated with each T-m(0) (not with a fixed T-m(0) for high-molecular-weight PLLA) decreased with increasing the amount of defects per unit mass of the polymer for crystallization, i.e. with increasing the comonomer content and the density of terminal group through decreasing the molecular weight. (c) 2005 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available