Soot oxidation over NOx storage catalysts:: Activity and deactivation

Journal

CATALYSIS TODAY
Volume 114, Issue 1, Pages 48-56

Publisher

ELSEVIER
DOI: 10.1016/j.cattod.2006.02.009

Keywords

soot oxidation; filter regeneration; NSR catalysts

Ask authors/readers for more resources

Soot oxidation activity and deactivation of NO, storage and reduction (NSR) catalysts containing Pt, K, and Ba supported on Al2O3, are studied under a variety of reaction conditions. K-containing catalysts decrease soot oxidation temperature with O-2 alone and the presence of Pt further enhance the activity due to synergetic effect. The active species responsible for synergism on Pt/K-Al2O3 are unstable and cannot be regenerated. Soot oxidation temperature decreases by about 150 degrees C with NO + O-2 exhaust feed gas and under lean conditions NSR system acts as catalysed soot filter (CSF). The reactions that are mainly responsible for decreasing soot oxidation temperature are: (i) soot oxidation with NO2 followed by NO recycles to NO2, and (ii) soot oxidation with O-2 assisted by NO2. Only a part of the stored NO, that is decomposed at high temperatures under lean conditions is found to be useful for soot oxidation. NO, storage capacity of NSR catalysts decreases upon ageing under soot oxidising conditions. This will lead to a decreased soot oxidation activity on stored nitrate decomposition. Pt/K-Al2O3 catalyst is more active, but least stable compared with Pt/Ba-Al2O3. (c) 2006 Elsevier B.V. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available