Preparation and electrorheological properties of triethanolamine-modified TiO2

Journal

JOURNAL OF SOLID STATE CHEMISTRY
Volume 179, Issue 5, Pages 1565-1568

Publisher

ACADEMIC PRESS INC ELSEVIER SCIENCE
DOI: 10.1016/j.jssc.2006.01.078

Keywords

electrorheological fluids; molecular dipole moment

Ask authors/readers for more resources

The high molecular dielectric dipole moment of doping material is promising, to improve the electrorholegical (ER) effect. It is found that triethanolamine (the molecular dipole moment of triethanolamine is 3,48)-modified TiO2 has good ER properties. Under 5 kV/mm external electric field. the yield stress is 32.6 kPa, which is about 50 times higher than that of TiO2 and the leaking electric current density is lower than 16 mu A/cm(3). The sedimentation rate is about 98% in 20 days. (C), 2006 Elsevier Inc. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.6
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available