Siderite (FeCO3) is commonly found in coal overburden and, when present, can cause interference in the determination of neutralization potential (NP). Under acidic testing conditions, FeCO3 reacts to neutralize acid, which. contributes to the NP. However, continued weathering of FeCO3 (oxidation of Fe2+ and hydrolysis of Fe3+) produces a neutral to slightly acidic solution. The effects of hydrogen peroxide (H2O2), potassium permanganate (KMnO4), and O-2 on the laboratory measurement of NP of siderite samples taken from overburden were examined. All oxidation treatments lowered the NP values of the siderite samples as compared with the standard USEPA method. However, oxidation with H2O2 produced variable results depending on the amount of H2O2 added. Neutralization potential values obtained after oxidation treatments were highly correlated with Mn concentration. Reaction products (i.e., 2-line ferrihydrite) of siderite samples with H2O2 and KMnO4 were not representative of natural siderite weathering. Oxidation with O-2 produced the lowest NP values for siderite samples. The reaction products produced by oxidation with O-2 most closely represent those intermediate products formed when siderite is exposed to atmospheric weathering conditions. Oxidation with O-2 also proved to be the most reproducible method for accurately assessing NP when siderite is present in overburden samples.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.4
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available