4.6 Article

Clinical performance of posterior metal-free polymer crowns with and without fiber reinforcement - One-year results of a randomised clinical trial

Journal

JOURNAL OF DENTISTRY
Volume 34, Issue 10, Pages 757-762

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/j.jdent.2006.02.001

Keywords

reinforced; non-reinforced; posterior; polymer; crowns; clinical; randomised; plaque; gingival index

Ask authors/readers for more resources

Objectives: The aim of this study was to evaluate the clinical performance of posterior, metal-free polymer crowns with and without a glass-fiber framework, in comparison to metal-ceramic crowns. Methods: After randomisation, 80 single crowns, manufactured from a newly designed polymer composite, were set in posterior teeth. Half of these received a glass-fiber framework, while half were prepared without any framework stabilisation. All polymer crowns were adhesively luted with resin cement. As the control group, 40 conventional metal-ceramic crowns were inserted with hybrid cement. Documentation included failures and other complications, as well as gingival/plaque status and aesthetic performance. Results: During the 12-month observation period, eight polymer crowns and three metal-ceramic crowns showed clinically relevant complications. The most frequent complications were root canal treatments (n = 4) and decementation (n = 4) of the crowns. A total of two crowns (one polymer crown with fiber network and one crown of the control group) had to be replaced. After 12 months, polymer crowns with glass-fiber framework exhibited significantly higher plaque accumulation (p = 0.005) and gingival index (p = 0.04) than metal-ceramic crowns, while no significant differences could be demonstrated for polymer crowns without fiber reinforcement. Postoperative sensibility and aesthetic performance did not differ significantly between the groups. Conclusions: Within a 12-month observation period, posterior polymer crowns with and without glass-fiber framework demonstrated acceptable stability and aesthetic performance. Polymer crowns with fiber framework showed significant higher plaque accumulation and gingival index than metal-ceramic crowns. (c) 2006 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.6
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available