Electrospinning of chitosan/poly(vinyl alcohol)/acrylic acid aqueous solutions

Journal

JOURNAL OF APPLIED POLYMER SCIENCE
Volume 102, Issue 6, Pages 5692-5697

Publisher

JOHN WILEY & SONS INC
DOI: 10.1002/app.25068

Keywords

chitosan; fibers; viscosity

Ask authors/readers for more resources

Chitosan bicomponent fibers were prepared via the electrospinning of chitosan/poly(vinyl alcohol)/acrylic acid aqueous solutions with different concentrations. With a 4% acrylic acid aqueous solution, when the chitosan/poly(vinyl alcohol) mass ratios were lower than 80/20, electrospinning nanofibers could be obtained. With a 90% acrylic acid aqueous solution, when the chitosan/poly(vinyl alcohol) mass ratios were less than 95/5, good nanofibers could be electrospun. The average diameter of the nanofibers gradually decreased, and its distribution became narrower as the poly(vinyl alcohol) concentration increased. Chitosan/poly(vinyl alcohol)/acrylic acid aqueous solutions could be electrospun at various concentrations by the adjustment of the chitosan and poly(vinyl alcohol) concentrations. The effects of the viscosity and conductivity of the blend solution on the morphologies of the fiber mats were also investigated. (c) 2006 Wiley Periodicals, Inc.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.6
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available