Volume 58, Issue 3, Pages 262-266Publisher
ELSEVIER SCIENCE INC
DOI: 10.1016/j.matchar.2006.05.001
Keywords
NiTi alloy; fatigue; laser welding; heat treatment; precipitate
Ask authors/readers for more resources
The influence of heat treatment on the rotating-bending fatigue of a laser-welded superelastic NiTi alloy wire was investigated. In comparison with the as-welded and annealed at 500 degrees C for 1 h specimens, the specimen annealed at 400 degrees C for 1 h shows the best fatigue resistance. The difference of fatigue life in the heat-treated materials is attributed to the different Ti3Ni4 precipitate size. Heat treatment to produce smaller coherent precipitates (10 nm) improves the fatigue resistance of the laser-welded NiTi alloy wire. When the Ti3Ni4 precipitates become coarse, the fatigue resistance decreases. (c) 2006 Elsevier Inc. All rights reserved.
Authors
I am an author on this paper
Click your name to claim this paper and add it to your profile.
Reviews
Recommended
No Data Available