Uranyl ion-imprinted polymeric (IIP) resins were prepared by dissolving stoichiometric amounts of uranyl nitrate and selected chelating ligands, viz. salicylaldoxime, catechol, succinicacid, 5,7-dichloroquinoline-8-ol and 4-vinyl pyridine in 2-methoxy ethanol (porogen) and copolymerizing thermally in the presence of 2-hydroxyethylmethacrylate (HEMA) and ethyleneglycol-dimethacrylate (EGDMA), using 2,2'-azobisisobutyronitrile (initiator). Again, IIP resins were also prepared on similar lines by utilizing ternary [uranium-non-vinylated ligand-vinylated ligand (4-vinyl pyridine)] complexes. Non-imprinted polymeric resins were identically prepared in both cases without the use of uranyl imprint ion. The percent enrichment and retention capacity studies showed significant imprinting effect in all cases. However, ion-imprinted polymeric resins formed with succinic acid (SA) or 5,7-dichloroquinoline-8-ol (DCQ) and 4-vinylpyridine (VP) alone gave quantitative enrichment and various parameters that influence the enrichment and elution were then optimized. The percent enrichment of uranium from synthetic seawater solutions was found to be 25.0 +/- 0.5 and 83.0 +/- 0.8 for SA-VP and DCQ-VP systems, respectively. The DCQ-VP-based IIP resins were successfully tested for the recovery of uranium from real seawater samples. (c) 2007 Elsevier B.V All rights reserved.
Authors
I am an author on this paper
Click your name to claim this paper and add it to your profile.
Reviews
Recommended
No Data Available