Piezoelectric, dielectric, and ferroelectric properties of 0-3 ceramic/cement composites

Journal

JOURNAL OF APPLIED PHYSICS
Volume 101, Issue 9, Pages -

Publisher

AMER INST PHYSICS
DOI: 10.1063/1.2730559

Keywords

-

Ask authors/readers for more resources

The sulphoaluminate cement and a piezoelectric ceramic, 0.08Pb(Li1/4Nb3/4)O-3 center dot 0.47PbTiO(3)center dot 0.45PbZrO(3)[P(LN)ZT], were used to fabricate 0-3 cement based piezoelectric composites. The piezoelectric, dielectric, and ferroelectric properties of the composites were mainly investigated. The results indicate that the piezoelectric strain factor d(33) increases as the P(LN)ZT volume fraction increases, which follows the cube model well. The dielectric constant epsilon(x) and dielectric loss tan delta show similar trends with the d(33). In the frequency range of 40-100 kHz, the dielectric constants of the composites decrease sharply, which is mainly attributed to interfacial polarization in the composite. Above 200 kHz, the cement-based piezoelectric composites exhibit good dielectric-frequency stability. Hysteresis measurements indicate that the composites exhibit typical ferroelectric hysteresis loops at room temperature. The remanent polarization P-r and the coercive field E-c of the composites increase as the P(LN)ZT volume fraction increases. Meanwhile, the remnant polarizations P-r shows little asymmetric characterization. (c) 2007 American Institute of Physics.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.6
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available