4.7 Article

Chemical durability studies of perfluorinated sulfonic acid polymers and model compounds under mimic fuel cell conditions

Journal

MACROMOLECULES
Volume 40, Issue 24, Pages 8695-8707

Publisher

AMER CHEMICAL SOC
DOI: 10.1021/ma071603z

Keywords

-

Ask authors/readers for more resources

Peroxide radical treatments of a perfluorinated ionomer used in polymer electrolyte membrane (PEM) fuel cells and its small molecule analogues were carried out, along with analysis of the resultant products. Molecules containing terminal carboxylic acids degraded at least 1 order of magnitude faster than noncarboxylate materials; all of the systems did show peroxide-initiated degradation nonetheless. Product analysis suggests that terminal carboxylic acids react according to a sequential chain shortening, consistent with previous studies. Cleavage of side chains from both polymer and model compounds was also observed to be important and in fact may be the dominate pathway in low carboxyl content commercial PEM membranes, based on the following comparison of reactivity and concentration. The relative reactivities of carboxylic chain ends and ether linkages is approximately 500, as calculated using model compounds fluoride generation rates. Commercial perfluorosulfonic acid (PFSA) products contain minimal carboxylic acid end groups, and the side chain concentrations are of 2-3 orders of magnitude higher than carboxylic acid end groups.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available