4.8 Article Proceedings Paper

Electrochemical properties of lithium sulfur cells using PEO polymer electrolytes prepared under three different mixing conditions

Journal

JOURNAL OF POWER SOURCES
Volume 174, Issue 2, Pages 745-750

Publisher

ELSEVIER
DOI: 10.1016/j.jpowsour.2007.06.108

Keywords

sulfur; polymer electrolyte; ball milling; lithium sulfur cell; Al2O3

Funding

  1. National IT Industry Promotion Agency (NIPA), Republic of Korea [C1090-0603-0023] Funding Source: Korea Institute of Science & Technology Information (KISTI), National Science & Technology Information Service (NTIS)

Ask authors/readers for more resources

Lithium sulfur cells were prepared by composing with sulfur cathode (PEO)(6)LiBF4 polymer electrolyte and lithium anode. (PEO)(6)LiBF4 polymer electrolyte was prepared under three different mixing conditions: stirred polymer electrolyte (SPE), ball-milled polymer electrolyte (BPE) and ball-milled polymer electrolyte with 10 wt%Al2O3 (BCPE). The effects of ball milling and additive were investigated by discharge test according to depth of discharge. The initial discharge capacity of lithium sulfur cell using BCPE was 1670 mAh g(-1)-sulfur, which was better than those of SPE and BPE, and approximately equal to the theoretical capacity. The cycle performance of Li/(PEO)(6)LiBF4/S cell was remarkably improved by the addition of Al2O3. (C) 2007 Elsevier B.V. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.8
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available