4.8 Article

Unentangled Star-Shape Poly(ε-caprolactone)s as Phthalate-Free PVC Plasticizers Designed for Non-Toxicity and Improved Migration Resistance

Journal

ACS APPLIED MATERIALS & INTERFACES
Volume 6, Issue 14, Pages 11118-11128

Publisher

AMER CHEMICAL SOC
DOI: 10.1021/am500740v

Keywords

endocrine disruptor; flexible PVC; migration; plasticizer; star-shape poly(epsilon-caprolactone)

Funding

  1. Industrial Strategic Technology Development Program - Ministry of Trade, Industry and Energy, Republic of Korea
  2. Korea Evaluation Institute of Industrial Technology (KEIT) [10035373] Funding Source: Korea Institute of Science & Technology Information (KISTI), National Science & Technology Information Service (NTIS)

Ask authors/readers for more resources

We develop a nontoxic unentangled star-shape poly(e-caprolactone) (UESPCL) plasticizer with excellent migration resistance for the production of phthalate-free flexible poly(vinyl chloride) (PVC) by means of the ring-opening polymerization of e-caprolactone, initiated from the multifunctional core, combined with end-capping, and vacuum purification processes. UESPCL is a transparent liquid at room temperature and exhibits unentangled Newtonian behavior because of its extremely short branched segments. UESPCL is biologically safe without producing an acute toxicity response. Torque analysis measurements reveals that UESPCL offers a faster fusion rate and a higher miscibility with PVC compared to a typical plasticizer, di(2-ethylhexyl phthalate (DEHP). The solid-state H-1 nuclear magnetic resonance (NMR) spectrum reveals that PVC and UESPCL are miscible with an average domain size of less than 8 nm. The flexibility and transparency of the PVC/UESPCL mixture, that is, phthalate-free flexible PVC, are comparable to the corresponding properties of the PVC/DEHP mixture, and the stretchability and fracture toughness of PVC/UESPCL are superior to the corresponding properties of the PVC/DEHP system. Most of all, PVC/UESPCL shows excellent migration resistance with a weight loss of less than 0.6% in a liquid phase, whereas DEHP migrated out of PVC/DEHP into a liquid phase with a weight loss of about 10%.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.8
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available