4.8 Article

Discrepancy of Optimum Ratio in Bulk Heterojunction Photovoltaic Devices: Initial Cell Efficiency vs Long-Term Stability

Journal

ACS APPLIED MATERIALS & INTERFACES
Volume 5, Issue 5, Pages 1612-1618

Publisher

AMER CHEMICAL SOC
DOI: 10.1021/am302185f

Keywords

organic solar cells; degradation; stability; bulk heterojunction; morphology; lifetime

Funding

  1. NRF
  2. Korea MEST [NRF-2009-C1AAA001-2009-0094157]
  3. NCRC program [2011-0006268, 2009-0092950]
  4. Global Frontier RD Program [2011-0031565]
  5. New and Renewable Energy Program through the KETEP
  6. Ministry of Knowledge Economy (MKE) [008NPV08J010000]

Ask authors/readers for more resources

Organic photovoltaic devices are difficult to commercialize because of their vulnerability to chemical degradation related with oxygen and water and to physical degradation with aging at high temperatures. We investigated the photophysical degradation behaviors of a series of poly(3-hexylthiophene) (P3HT)/[6,6]-phenyl C61-butyric acid methyl ester (PC60BM) bulk heterojunctions (BHJs) as a model system according to the donor-acceptor ratio. We found that the optimum P3HT:PC60BM ratio in terms of long-term stability differs from that in terms of initial cell efficiency. On the basis of cell performance decays and time-resolved photoluminescence measurements, we investigated the effects of oxygen and material self-aggregation on the stability of an organic photovoltaic device. We also observed the changes in morphological geometry and analyzed the surface elements to verify the mechanisms of degradation.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.8
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available