4.7 Article

Novel insight into evolution mechanism of second liquid-liquid phase separation in metastable immiscible Cu-Fe alloy

Journal

MATERIALS & DESIGN
Volume 156, Issue -, Pages 71-81

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/j.matdes.2018.06.044

Keywords

Phase separation; Morphological pattern; Minority phase; Phase field simulation

Funding

  1. National Key Research and Development Program of China [2017YFA0403802, 2017YFB0306105, 2016YFB0301303]
  2. National Natural Science Foundation of China [51771040, 51501028, 51690163, 51525401]
  3. Fundamental Research Funds for the Central Universities of China [DUT17JC44]

Ask authors/readers for more resources

The metastable immiscible Cu80Fe20 alloys with different diameters were systematically investigated under conventional solidification. Experimental results indicated that the primary and second liquid-liquid phase separation simultaneously occur during solidification. The average size of primary phase-separated Fe-rich spherulites and the interior morphological pattern of minority Cu-rich phase can be greatly influenced by cooling rate due to the dynamic coupling between thermodynamic and kinetic effects. Moreover, various morphological patterns of minority Cu-rich phase in Fe-rich spherulites were observed, which discloses the dynamic evolution process during self-driven second liquid-liquid phase separation. The Marangoni migration, coalescence and coagulation, and Ostwald ripening are the dynamic mechanisms mainly responsible for various morphological patterns of minority Cu-rich phase after phase separation. Such a clear experimental observation of dynamic microstructure evolution for minority Cu-rich phase provides a strong and visualized evidence for the asynchronous crystallization behavior of primary phase-separated Fe-rich spherulites. Phase field simulation was also performed to reveal the dynamic evolution of minority Cu-rich phase during liquid-liquid phase separation. Besides, the experimental Cu80Fe20 alloys exhibit soft ferromagnetic characteristics possessing relatively low coercivity and high saturated magnetization. This present study provides a new strategy to design immiscible alloy with anticipated microstructure possessing tailored properties and desired functionalities. (C) 2018 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available