3.8 Proceedings Paper

Dyeing Properties of Acetylated Wood with Red Disperse Dyes

Journal

ADVANCED MATERIALS AND STRUCTURES, PTS 1 AND 2
Volume 335-336, Issue -, Pages 1061-1066

Publisher

TRANS TECH PUBLICATIONS LTD
DOI: 10.4028/www.scientific.net/AMR.335-336.1061

Keywords

Acetylated Wood; Wood dyeing; Percentage of dye exhaustion; Color difference; Color fastness to washing

Ask authors/readers for more resources

The dyeing properties of acetylated fir powder and acetylated poplar spill with 8 red disperse dyes were studied in this paper. The dyeing results indicate that the percentage of dye exhaustion (% E)on acetylated fir powder is 96 similar to 99%. As for acetylated poplar spill, the percentage of dye exhaustion reaches 58 similar to 78%. The color shade of dyed modified wood is similar to that of dyed polyester fabric. Compared with the dyed polyester fabric, the color difference(Delta E) of dyed modified wood is smaller than that of dyed unmodified wood under the same dyeing conditions. Furthermore, modified fir powder has excellent color fastness to washing, the dye removal of dyed acetylated fir powder is 0.4 similar to 1.8% at 80 degrees C for 2 h in the water. Both the Infrared (IR) spectra and microscopic images of fir powder, acetylated fir powder and dyed acetylated fir powder were investigated.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

3.8
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available