Hydrogenation of Anthracene and Dehydrogenation of Perhydroanthracene on Pt/C Catalysts

Journal

RUSSIAN JOURNAL OF PHYSICAL CHEMISTRY A
Volume 92, Issue 4, Pages 663-668

Publisher

MAIK NAUKA/INTERPERIODICA/SPRINGER
DOI: 10.1134/S0036024418040106

Keywords

catalysis; hydrogenation of anthracene; dehydrogenation of perhydroanthracene

Ask authors/readers for more resources

The hydrogenation of anthracene on a heterogeneous catalyst containing 3 wt % Pt/C (Aldrich) at 215, 245, and 280A degrees C and the pressures of 40 and 90 atm is studied. The hydrogenation of anthracene to a completely hydrogenated product is considered in detail. The final product (perhydroanthracene) consists of five conformational isomers with total selectivity of more than 99%. The ratio of perhydroanthracene isomers in the end product is shown to be determined by the conditions (P, T) of hydrogenation. The rate of hydrogenation is found to slow upon an increase in the degree of benzene ring saturation. A mixture of perhydroanthracene isomers is dehydrogenated in an autoclave at 260-325A degrees C on 3 wt % Pt/C catalyst (Aldrich) and in a flow reactor at 300-360A degrees C on 3 wt% Pt/Sibunit catalyst. The reactivity of perhydroanthracene isomers in dehydrogenation is shown to differ.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.2
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available