Tensile behavior of C fiber reinforced amorphous SiCN ceramic matrix composites (C/SiCN) were investigated by tensile machine. The microstructure morphologies were observed by scanning electron microscope. The results indicate that the tensile stress-strain curves of C/SiCN composites dispaly typical elastic deformation and cracks propagation stages. The 1500 degrees C pre-sabilization treatment of C/SiCN in vacuum facilitates room temperature tensile stress growth. The higher treated temperature such as 1900 degrees C is yet opposite. The reasons were attributed to thermal stress relaxation of C/SiCN after pre-stabilization treatment in vacuum.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

3.8
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available