THE PROPERTIES OF 3 nm-SIZED DETONATION DIAMOND FROM THE POINT OF VIEW OF COLLOID SCIENCE

Journal

UKRAINIAN JOURNAL OF PHYSICS
Volume 60, Issue 9, Pages 932-937

Publisher

BOGOLYUBOV INST THEORETICAL PHYSICS NATL ACAD SCI UKRAINE
DOI: 10.15407/ujpe60.09.0932

Keywords

detonation nanodiamonds; hydrosol; regularities of coagulation; origin of the particle charge; transmission electron microscopy; dynamic light scattering; size-concentration dependence

Ask authors/readers for more resources

The colloidal properties of the hydrosol of a detonation nanodiamond have been considered and discussed. The 3nm-sized positively charged colloidal species produced by the NanoCarbon Research Institute, Japan, undergo a further aggregation on the dilution. They exhibit the emission at 625 nm with the excitation maximum at 491 nm, adsorb anionic dyes, and readily coagulate at the adding of electrolytes. The coagulation occurs in line with the Schulze-Hardy rule, the coagulation strength of the anions follows the Hofmeister series, whereas the abnormally high influence of the most hydrophilic anion, HO-, allows revealing the acidic character of the positive surface charge. The hypothesis of the so-called periodic colloidal structures has been put forward in order to explain the dependence of the particle size on the concentration of the hydrosol and the high viscosity of the initial 5.0 wt./vol. % detonation nanodiamond colloid.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

3.8
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available