3.8 Article

Use of aluminium alkoxide and oxazolidine II to treat acid-deteriorated historic leather

Journal

JOURNAL OF THE INSTITUTE OF CONSERVATION
Volume 38, Issue 2, Pages 172-187

Publisher

ROUTLEDGE JOURNALS, TAYLOR & FRANCIS LTD
DOI: 10.1080/19455224.2015.1071713

Keywords

leather; conservation; acid deterioration; red rot; artificial ageing; shrinkage temperature

Ask authors/readers for more resources

This study was undertaken to develop a product that will potentially delay the progress of deterioration of acid-deteriorated historic leather. Acid-deteriorated leather samples were treated with a new formulation consisting of aluminium di(isopropoxide) acetoacetate ester chelate (aluminium alkoxide) and 5-ethyl-1-aza-3,7-dioxabicyclo-[3.3.0]octane (oxazolidine II). The leather samples were also treated with oxazolidine II and aluminium alkoxide separately to compare the effectiveness of these reagents against the new formulation. Untreated leather samples were used as a negative control. Acid-deteriorated leather samples treated with Cellugelw, aluminium alkoxide and the new formulation along with corresponding untreated leather samples were also subjected to accelerated ageing in order to investigate the longevity of the treated leather. The impact of the treatments and accelerated ageing was determined by measuring the hydrothermal stability of the leather and pH of the aqueous extract. The formulation showed a potential to provide the acid-deteriorated historic leather with long-term protection against an artificially-created acidic environment.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

3.8
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available