The dynamics of Fe oxidation in riebeckite: A model for amphiboles

Journal

AMERICAN MINERALOGIST
Volume 103, Issue 7, Pages 1103-1111

Publisher

MINERALOGICAL SOC AMER
DOI: 10.2138/am-2018-6382

Keywords

Riebeckite; HT spectroscopy; FTIR; Raman; iron oxidation; deprotonation

Funding

  1. Deutsche Forschungsgemeinschaft [1127/7-2]

Ask authors/readers for more resources

In this work, we investigate the oxidation behavior of a nearly end-member riebeckite, ideally Na-2(Fe32+Fe23+)Si8O22(OH)(2), by using vibrational FTIR and Raman spectroscopies. Combining these results with previous studies performed on the same sample by single-crystal structure refinement and Mossbauer spectroscopy, we conclude that iron oxidation in riebeckite is a multi-step process. (1) In the similar to 523 K < T < 623 K temperature range, the O-H bond lengthens and both the electrons and the hydrogen cations delocalize. Raman analysis shows that this step is reversible upon cooling to room temperature. (2) In the 623 K < T < 723 K range, the kinetic energy increases so that the electrons can be ejected from the crystal; beyond 723 K an irreversible oxidation of Fe occurs that couples with irreversible changes in the SiO4 double-chains leading to a contraction of the unit-cell volume, i.e., to structural changes detectable at the long-range scale. (3) Beyond 823 K, the irreversible oxidation is completed and H+ ions are forced to leave the crystal bulk. Because of this multi-step process, the onset of the deprotonation process is detected at similar to 700 K by single-crystal XRD analysis of the unit-cell parameters, but starts at 623 K as indicated by Mossbauer spectroscopy on powders (and by changes in the cation distribution observed by structure refinement). Also, Raman scattering shows that the release of H+ from the crystal surface starts similar to 100 K before the complete deprotonation of the crystal bulk is witnessed by FTIR absorption. Hence, the oxidation of Fe starts at the crystal surface and induces electron and H+ migration from the crystal interior to the rim and thus subsequent oxidation through the crystal bulk. No deprotonation is observed by FTIR either in powders embedded in KBr or in crystals heated in N-2 atmosphere, implying that the release of H+ needs surficial (atmospheric) oxygen to form H2O molecules. Fe2+-> Fe3+ oxidation produces a flux of electrons throughout the crystal matrix, which generates electrical conductivity across the amphibole. An important implication of this work, which might have interesting applications in material science, is that iron oxidation in riebeckite (and possibly in other Fe-rich silicates) is reversible in a given range of temperature. Also, this work shows that complex processes cannot be fully understood or even monitored accurately without using a proper combination of independent techniques.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.5
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available