4.3 Article

Enhancement of photocatalytic degradation of organic dyes using ZnO decorated on reduced graphene oxide (rGO)

Journal

DESALINATION AND WATER TREATMENT
Volume 108, Issue -, Pages 311-321

Publisher

DESALINATION PUBL
DOI: 10.5004/dwt.2018.21947

Keywords

ZnO/rGO; Characteristics; Photocatalytic degradation; Congo red; Reaction kinetic

Funding

  1. Fundamental Research Grant Scheme by the Ministry of Education (MOE) Malaysia
  2. Universiti Tunku Abdul Rahman Research Grant through the Centre for Photonics and Advanced Materials Research
  3. Universiti Tunku Abdul Rahman Research Grant through the Centre for Environment and Green Technology (CEGT), UTAR

Ask authors/readers for more resources

Reduced graphene oxide (rGO) with excellent electron capturing ability could be coupled with semiconductor photocatalyst to prevent the recombination problem of photogenerated hole-electron pairs encountered by pure zinc oxide (ZnO) while simultaneously promote the photocatalytic activity. In this study, rGO decorated with ZnO (ZnO/rGO) photocatalyst was synthesized for the photocatalytic degradation of rhodamine B, congo red and methyl orange in water. The ZnO and ZnO/rGO photocatalysts were characterized by using field emission scanning microscopy-energy dispersive X-ray analysis and X-ray powder diffraction, and Fourier transformed infrared spectroscopic analyses. The morphology and elemental results showed that both catalysts were in spherical shape and free from impurities. It was found that the average particle size of ZnO/rGO was smaller than that of pure ZnO which indicated that ZnO decorated on graphene sheet would decrease the particle size. Congo red showed the highest degradation efficiency and it was attributed to the rapid break down of its azo bond (-N=N-) and aromatic rings by hydroxyl radicals. It was found that 97.96% degradation could be achieved in 1 h under optimum conditions which were at 10 mg/L of initial congo red concentration, 2 g/L of ZnO/rGO catalyst dosage and a solution pH of 7. The spent ZnO/rGO exhibited high catalytic activity of 96.67% at optimum conditions indicating its high stability to act as a photocatalyst. The photocatalytic degradation of congo red satisfactorily fitted a pseudo-first-order reaction kinetic. Besides, the removal of chemical oxygen demand for congo red after 1 h of photocatalytic degradation was nearly 100%.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.3
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available