4.6 Article

Development of a cyan blue-emitting Ba3La2(BO3)4:Ce3+,Tb3+ phosphor for use in dental glazing materials: color tunable emission and energy transfer

Journal

RSC ADVANCES
Volume 11, Issue 40, Pages 24949-24957

Publisher

ROYAL SOC CHEMISTRY
DOI: 10.1039/d1ra04384f

Keywords

-

Funding

  1. Technology Development Program - Ministry of SMEs and Startups (MSS, Korea) [S2800580]
  2. Korea Technology & Information Promotion Agency for SMEs (TIPA) [S2800580] Funding Source: Korea Institute of Science & Technology Information (KISTI), National Science & Technology Information Service (NTIS)

Ask authors/readers for more resources

Ce3+/Tb3+ doped Ba3La2(BO3)(4) phosphors were synthesized by conventional solid state reaction. The optimized composition yielded a cyan-blue emission with high color purity, and the internal quantum efficiency was estimated to be 50%. A dental glazing paste prepared with organic binder, Ba3La2(BO3)(4):Ce3+,Tb3+ phosphors, and low T-g glass showed high chemical stability in acidic aqueous solution (pH = 4) and successfully vitrified at 600 and 700 degrees C.
The Ce3+/Tb3+ doped Ba3La2(BO3)(4) phosphors were synthesized by a conventional solid state reaction method. The synthesized phosphor samples are a single phase of Ba3La2(BO3)(4) and showed angular-shaped fine grains with average particle size from 5 mu m to 10 mu m. The Ba3La2(BO3)(4):Ce3+ phosphors showed an asymmetric broad blue emission under excitation at 365 nm and the Ba3La2(BO3)(4):Tb3+ phosphors exhibited typical green emission assigned to the 4f-4f transition of Tb3+ under excitation at 254 nm. Under near-UV (365 nm) excitation, Ba3La2(BO3)(4):Ce3+,Tb3+ phosphors showed both a blue emission band and green emission peaks due to Ce3+ and Tb3+, respectively. By optimizing the composition, cyan-blue emission with high color purity (CIE chromaticity coordinate values x = 0.2557 and y = 0.3839) was obtained for the Ba3La2(BO3)(4):0.05Ce(3+),0.03Tb(3+) phosphor, and the internal quantum efficiency of the phosphor at the excitation wavelength of 365 nm is estimated to be 50%. The dental glazing paste prepared by mixing organic binder, Ba3La2(BO3)(4):Ce3+,Tb3+ phosphors, and low T-g glass was successfully vitrified when it was heated at 600 and 700 degrees C, and showed high chemical stability of the luminescence properties in acidic aqueous solution (pH = 4).

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.6
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available