The study investigates the use of temporal and spatial power modulation in laser beam micro welding to achieve variable control of the weld penetration depth. The combined power modulation enables precise control of the welding depth in different material combinations.
For joining metallic materials for battery applications such as copper and stainless steel, laser beam micro welding with beam sources in the near-infrared range has become established in recent years. In laser beam micro welding, spatial power modulation describes the superposition of the linear feed motion with an oscillating motion. This modulation method serves to widen the cross-section of the weld seam as well as to increase the process stability. Temporal power modulation refers to the controlled modulation of the laser power over time during the welding process. In this paper, the superposition of both temporal and spatial power modulation methods is presented, which enables a variable control of the weld penetration depth. Three weld geometries transverse to the feed direction are part of this investigation: the compensation of the weld penetration depth due to the asymmetric path movement during spatial power modulation only, a W-shaped weld profile, and a V-shaped. The weld geometries are investigated by the bed on plate weld tests with CuSn6. Furthermore, the use of combined power modulation for welding tests in butt joint configuration between CuSn6 and stainless steel 1.4301 with different material properties is investigated. The study shows the possibility of precise control of the welding depth by this methodology. Depending on the material combination, the desired regions with maximum and minimum welding depth can be achieved by the control of local and temporal power modulation on the material surface.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.0
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available