4.7 Article

Synergistic effect of ultrasonic cavitation erosion and corrosion of WC-CoCr and FeCrSiBMn coatings prepared by HVOF spraying

Journal

ULTRASONICS SONOCHEMISTRY
Volume 31, Issue -, Pages 563-569

Publisher

ELSEVIER
DOI: 10.1016/j.ultsonch.2016.02.011

Keywords

HVOF; WC-CoCr; FeCrSiBMn; Corrosion; Cavitation; Synergism

Funding

  1. Natural Science Foundation of Jiangsu Province of China [BK20150806]
  2. National Natural Science Foundation of China [51131008, 51339005, 51579087]
  3. Fundamental Research Funds for the Central Universities [2015B01514]
  4. Key Laboratory of Nuclear Materials and Safety Assessment, CAS [2016NMSAKF03]

Ask authors/readers for more resources

The high-velocity oxygen-fuel (HVOF) spraying process was used to fabricate conventional WC-10Co-4Cr coatings and FeCrSiBMn amorphous/nanocrystalline coatings. The synergistic effect of cavitation erosion and corrosion of both coatings was investigated. The results showed that the WC-10Co-4Cr coating had better cavitation erosion-corrosion resistance than the FeCrSiBMn coating in 3.5 wt.% NaCl solution. After eroded for 30 h, the volume loss rate of the WC-10Co-4Cr coating was about 2/5 that of the FeCrSiBMn coating. In the total cumulative volume loss rate under cavitation erosion-corrosion condition, the pure cavitation erosion played a key role for both coatings, and the total contribution of pure corrosion and erosion-induced corrosion of the WC-10Co-4Cr coating was larger than that of the FeCrSiBMn coating. Mechanical effect was the main factor for cavitation erosion-corrosion behavior of both coatings.(C) 2016 Elsevier B.V. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available