alpha-MnO2 nanowires (NWs) prepared by hydrothermal method are characterized using XRD and FT-IR. The crystallite size, surface area of NWs increases, whereas dislocation density and band gap decreases with an increase in oxidizer molarity. The band gap decreases from 2.55 to 1.27 eV. The above observations correlate well with the enhanced catalytic activity of MnO2 NWs for degradation of azo dye reactive black 5 (RB5). About 70% of the dye were successfully removed in 60 min using 20 mg of MnO2 NWs in the presence of 6 mL of H2O2. MnO2 NWs show a good reusability, suggesting it as an effective and recyclable catalyst. (C) 2016 Elsevier B.V. All rights reserved.
Authors
I am an author on this paper
Click your name to claim this paper and add it to your profile.
Reviews
Recommended
No Data Available