Related references
Note: Only part of the references are listed.Effect of thermal cycling on protective properties of alumina scale grown on thin Haynes 214 foil
A. Chyrkin et al.
CORROSION SCIENCE (2015)
Influence of grain orientation on the incipient oxidation behavior of Haynes 230 at 900 °C
Xu Wang et al.
MATERIALS CHARACTERIZATION (2015)
Effects of Silicon on High Temperature Corrosion of Fe-Cr and Fe-Cr-Ni Alloys in Carbon Dioxide
Thuan Dinh Nguyen et al.
OXIDATION OF METALS (2014)
The effect of Mn1.5Co1.5O4 coatings on the development of near surface microstructure for Haynes 230 oxidized at 800 °C in air
Neal J. Magdefrau et al.
SURFACE & COATINGS TECHNOLOGY (2014)
Slow Transition from Protective to Breakaway Oxidation of Haynes 214 Foil at High Temperature
D. J. Young et al.
OXIDATION OF METALS (2013)
Hydrogen effects on oxidation behaviors of Haynes 230 in high temperature steam environments
Donghoon Kim et al.
SOLID STATE IONICS (2013)
High Temperature Materials Corrosion Challenges for Energy Conversion Technologies
Elizabeth Opila
ELECTROCHEMICAL SOCIETY INTERFACE (2013)
Incipient oxidation kinetics and residual stress of the oxide scale grown on Haynes 230 at high temperatures
Hsiao-Ming Tung et al.
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING (2012)
High-temperature oxidation performance of a new alumina-forming Ni-Fe-Cr-Al alloy in flowing air
V. P. Deodeshmukh et al.
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY (2011)
An Electron Microscopy Investigation of the Transient Stage Oxidation Products in an Fe-22Cr Alloy with Ce and La Additions Exposed to Dry Air at 1073 K (800 °C)
Jingxi Zhu et al.
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE (2011)
Oxidation Characteristics and Oxide Layer Evolution of Alloy 617 and Haynes 230 at 900 A°C and 1100 A°C
Daejong Kim et al.
OXIDATION OF METALS (2009)
The nature of the third-element effect in the oxidation of Fe-xCr-3 at.% Al alloys in 1 atm O2 at 1000 °C
Y. Niu et al.
CORROSION SCIENCE (2008)
Growth and adherence of chromia based surface scales on Ni-base alloys in high- and low-pO2 gases
J. Zurek et al.
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING (2008)
Correlation between the microstructure, growth mechanism, and growth kinetics of alumina scales on a FeCrAlY alloy
D. Naumenko et al.
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE (2007)
The role of silicon in the reactive-elements effect on the oxidation of conventional austenitic stainless steel
A. Paul et al.
OXIDATION OF METALS (2007)
Oxidation kinetics of Haynes 230 alloy in air at temperatures between 650 and 850°C
Li Jian et al.
JOURNAL OF POWER SOURCES (2006)
Criteria for the formation of protective Al2O3 scales on Fe-Al and Fe-Cr-Al alloys
ZG Zhang et al.
CORROSION SCIENCE (2006)
Influence of preoxidation and annealing treatments on the isothermal oxidation in air at 1173 K of cerium-implanted EN-1.4301 stainless steel
A Paúl et al.
OXIDATION OF METALS (2002)