Predicting the performance of existing pre-cast concrete pipes using destructive and non-destructive testing techniques

Journal

HELIYON
Volume 9, Issue 5, Pages -

Publisher

CELL PRESS
DOI: 10.1016/j.heliyon.2023.e15471

Keywords

Condition assessment; Precast concrete pipe; Non-destructive test (NDT); Destructive test

Ask authors/readers for more resources

The sewer pipeline network and water distribution system are vital urban assets for a sustainable community. Continuous evaluation of the condition of water and sewer concrete pipelines is essential to ensure reliable and cost-efficient transport of water and sewerage. Currently, the assessment is done through visual observations and non-destructive testing methods, but there is a need to shift to advanced assessment techniques.
One of the most significant and critical urban assets for a sustainable community is the sewer pipeline network and water distribution system. Water sewer networks and distribution systems have a definite service life span to provide continuous facilities to end users. Therefore, it is pertinent to continuously evaluate the condition of water and sewer concrete pipelines to ensure the reliable, sustainable, and cost-efficient transport of water and sewerage for the safety of society. The condition assessment is commonly carried out by visual observations followed by some non-destructive testing methods. However, it is the need of the hour to shift assessment methods to advance assessment techniques to save time and money for our community. Currently, in this project, the condition assessment of pre-cast concrete pipes was carried out by destructive and non-destructive methods. Different test trials i.e., ultra-sonic pulse velocity, Schmidt hammer also known as rebound hammer test, visual inspection, three edge bearing test, and core cutting test on the old buried and new concrete pipes were performed. It was observed that concrete used for the construction of existing precast concrete pipes still has better quality indices after 20 years as compared to that of concrete of new pipes. However, steel has deteriorated with time and clear corrosion of steel was identified in existing pre-cast concrete pipes. At the same time, it was observed that there should be an automated mechanism to continuously asses the condition of pre-cast existing pipes which will address the sustainable development goals (SDG 6, 9, 11). Consequently, it can be said that condition assessment of pre-cast concrete pipes will lead to sustainable societies and infrastructure.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.5
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available