In this study, the mechanical, wear, fracture toughness, drop load impact, and hydrophobicity behavior of the kevlar/sisal fiber composite laminates with cellulose addition were examined. The results showed that composite designation C3 exhibited the highest improvement in mechanical properties, while composite designation C4 had the lowest wear rate and coefficient of friction. Additionally, the addition of cellulose and the fiber stacking order influenced higher penetration resistance in drop load impact toughness.
This study examined the inter-ply alternatively stacked kevlar/sisal fiber's mechanical, wear, fracture toughness, drop load impact, and hydrophobicity behavior along with cellulose addition. This study also gives an insight to how effectively a biomass-derived fiber is used as potential replacement for synthetic man-made hazardous fibers. The composite laminates were made by room temperature hand layup process and hot cured at 120 degrees C for 2 h. The laminated composites are then subjected to testing in accordance to respective ASTM standards. The result finding reveals that the composite designation C3 possessed highest improvement in mechanical properties. Similarly, in wear, the composite designation C4 records a lowest sp. wear rate and COF of 0.011 mm(3)/Nm and 0.34. Moreover, in fracture toughness, the composite designation C3 scored a maximum fracture toughness of 24.74 (K(1)c) MPa. vm and energy release rate of 0.55 (G1c) MJ/m(2). This is about 339.43% and 223.52% of improvement compared to the plain resin. Similarly, in drop load impact toughness, the addition of cellulose and fiber stacking order influenced higher penetration resistance. Moreover, there is a strong matrix-fiber adhesion which causes finely fragmented fibers, which are visible through SEM fractography. Finally, the water-absorption behavior proves that composite materials' hydrophobicity has been maintained not less than 70 degrees despite the addition of cellulose and fiber. These composites, with improved load bearing effect with novel stacking order, could be benefited in manufacturing of building materials, automotive parts, aircraft bodies, and defense gadgets.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.5
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available