4.7 Article

Effect of pre-oxidation treatment on the bonding strength and thermal shock resistance of SiC coating for C/C-ZrC-SiC composites

Journal

CERAMICS INTERNATIONAL
Volume 41, Issue 5, Pages 6956-6964

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/j.ceramint.2015.01.151

Keywords

C/C-ZrC-SiC composites; Pre-oxidation treatment; Bonding strength; Thermal shock

Funding

  1. National Natural Science Foundation of China [51221001, 51222207]
  2. Research Fund of the State Key Laboratory of Solidification Processing (NWPU), China [12-BZ-2014]

Ask authors/readers for more resources

To improve the bonding strength and thermal shock resistance of SiC coating for C/C-ZrC-SiC composites, a transition layer with mechanical interlocking structure was constructed at the interface by pre-oxidation treatment and chemical vapor deposition. For the coated specimens with pre-oxidation treatment at 1073 K for 5 min, the bonding strength increased from 2.0 to 4.0 N, and the mass loss percentage decreased by 52.5% after 12-time thermal cycling between 1773 K and room temperature in air. The transition interlocking structure can effectively alleviate the mismatch between the coefficients of thermal expansion of SiC coating and C/C-ZrC-SiC substrate, improving the bonding strength and thermal shock resistance. As the pre-oxidation time increases, a rugged and loose ZrO2-SiO2 layer will be formed at the interface, which is disadvantageous to the bonding strength and thermal shock resistance of SiC coating for C/C-ZrC-SiC composites, and results in the debonding and collapse of the coating. (C) 2015 Elsevier Ltd and Techna Group S.r.l. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available