(Ta,W)C ceramic bulks were prepared by spark plasma sintering. The densification kinetics and solid-solution formation kinetics of the powder mixtures using TaC and W powders were studied. It was found that sintering at 2000 degrees C limits the reaction volume and allows forming a complete solid-solution using finer powders. The flexural strength of the (Ta,W)C ceramic bulks was investigated as a function of the TaC content, and the maximum strength was found for the 60 mol.% TaC composition. Strength increased up to 1200 degrees C and then gradually decreased to 2000 degrees C. When TaC was reinformed by coarse W spheres, the flexural strength decreased from 570 MPa at room temperature to 220 MPa at 2000 degrees C.
(Ta,W)C bulks were prepared by spark plasma sintering. Densification kinetics and solid-solution formation kinetics were performed on the powder mixtures using TaC and W powders. The as-received tungsten powder had a spherical shape and rather coarse size. By using the crushed and as-received powder, it can be suggested that sintering at 2000 degrees C limits the reaction volume to 3-6 mu m and hence allows forming a complete solid-solution using finer powders. The lattice parameter, hardness, toughness, and strength were investigated as a function of the TaC content. The flexural strength of the (Ta,W)C ceramic bulks was investigated up to 2000 degrees C and it was found that the maximum strength was for the 60 mol.% TaC composition. Strength as a function of the temperature tended to increase up to 1200 degrees C followed by a gradual decrease to 2000 degrees C. When the TaC was reinformed by coarse W spheres, the flexural strength monotonically decreased from 570 MPa at room temperature to 220 MPa at 2000 degrees C.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.5
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available