4.7 Article

Rheology, durability, and mechanical performance of sustainable self-compacting concrete with metakaolin and limestone filler

Journal

CASE STUDIES IN CONSTRUCTION MATERIALS
Volume 17, Issue -, Pages -

Publisher

ELSEVIER
DOI: 10.1016/j.cscm.2022.e01143

Keywords

Supplementary cementitious materials; Material efficiency; Plastic viscosity; Yield stress; Resistivity; Ultrasonic pulse velocity

Funding

  1. MINECO [BIA2014-58063-R, BIA2017-85657-R, BES-2015-071919]
  2. FPI 2015
  3. IACOBUS program for Galicia-North of Portugal Euroregion

Ask authors/readers for more resources

This study analyzed the performance and hardened properties of self-compacting concrete with different binder compositions and materials. The results showed that substituting cement with limestone filler and metakaolin can improve the rheological properties of the concrete while affecting the strength and resistivity. Self-compacting concrete with ternary binders demonstrated the highest performance.
This study analyzed the performance of self-compacting concrete with a paste composition that includes limestone filler and metakaolin replacing cement to design binary (75% cement and 25% limestone filler) and ternary binders (60% cement, 25% limestone filler and 15% metakaolin). Furthermore, to analyze the effect of the solid volume fraction (volume of sand and coarse aggregate) on concrete rheology, the concretes were designed using four volumes of paste (350 l, 400 l, 450 l and 500 l). Rheological tests were performed at three resting times to measure the viscosity and yield stress over time. The results indicated that the viscosity decreased by 43.3% when the cement was replaced by limestone filler and increased by 73.1% when the cement was replaced by 15% metakaolin while maintaining the limestone filler. These values were obtained as 27.6% and 62.2%, respectively, when the yield stress was analyzed. In addition, the hardened properties (mechanical behavior and durability) were studied by measuring the strengths at 28 days, as well as the electrical resistivity and ultrasonic pulse velocity over time. In this case, at 28 days the use of binary binder reduces the strength and resistivity (about 20%) and the employment of ternary binder reduces strength (15%) while increases the resistivity up to the double (when compared to the 100 C concrete). Moreover, to measure the efficiency of the concrete, a material index was designed that considers the fresh behavior, mechanical performance, durability, cost, and environmental impact. Self-compacting concretes with ternary binders provided the highest indices. The use of alternative materials, particularly metakaolin has been proven to be a good option to enhance concrete sustainable performance.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available