4.7 Article

Different coatings on magnetic nanoparticles dictate their degradation kinetics in vivo for 15 months after intravenous administration in mice

Journal

JOURNAL OF NANOBIOTECHNOLOGY
Volume 20, Issue 1, Pages -

Publisher

BMC
DOI: 10.1186/s12951-022-01747-5

Keywords

Iron oxide nanoparticle; Surface coating; Biodegradation; Biodistribution; Biotransformation

Funding

  1. CRUE-CSIC
  2. Springer Nature
  3. MCIN/AEI [SAF2017-82223-R, PID2020-112685RB-100, PGC2018-096016-B-I00, IJCI-2017-31447]
  4. ERDF a way of making Europe
  5. predoctoral FPU grant (MCIN/AEI) [FPU15/06170]
  6. predoctoral FPU grant (ESF Investing in your future)
  7. Santander-Universidad Zaragoza Fellowship program
  8. Nanomedicine CSIC HUB [202180E048]

Ask authors/readers for more resources

This study analyzed the biodistribution, organ accumulation and degradation of different coatings of iron oxide magnetic nanoparticles (MNPs) in vivo. The results showed that the coating influenced the proportion of MNPs in different organs, with faster degradation in the liver regardless of the coating. This information is important for choosing the optimal coating for specific biomedical applications.
Background: The surface coating of iron oxide magnetic nanoparticle (MNPs) drives their intracellular trafficking and degradation in endolysosomes, as well as dictating other cellular outcomes. As such, we assessed whether MNP coatings might influence their biodistribution, their accumulation in certain organs and their turnover therein, processes that must be understood in vivo to optimize the design of nanoformulations for specific therapeutic/diagnostic needs. Results: In this study, three different MNP coatings were analyzed, each conferring the identical 12 nm iron oxide cores with different physicochemical characteristics: 3-aminopropyl-triethoxysilane (APS), dextran (DEX), and dimercaptosuccinic acid (DMSA). When the biodistribution of these MNPs was analyzed in C57BL/6 mice, they all mainly accumulated in the spleen and liver one week after administration. The coating influenced the proportion of the MNPs in each organ, with more APS-MNPs accumulating in the spleen and more DMSA-MNPs accumulating in the liver, remaining there until they were fully degraded. The changes in the physicochemical properties of the MNPs (core size and magnetic properties) was also assessed during their intracellular degradation when internalized by two murine macrophage cell lines. The decrease in the size of the MNPs iron core was influenced by their coating and the organ in which they accumulated. Finally, MNP degradation was analyzed in the liver and spleen of C57BL/6 mice from 7 days to 15 months after the last intravenous MNP administration. Conclusions: The MNPs degraded at different rates depending on the organ and their coating, the former representing the feature that was fundamental in determining the time they persisted. In the liver, the rate of degradation was similar for all three coatings, and it was faster than in the spleen. This information regarding the influence of coatings on the in vivo degradation of MNPs will help to choose the best coating for each biomedical application depending on the specific clinical requirements.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available