4.7 Article

Near-net shaping of laminated Al/Al2O3 composites by direct ink writing and pressure infiltration

Publisher

ELSEVIER SCIENCE SA
DOI: 10.1016/j.msea.2022.144267

Keywords

3-D printing; Pressure infiltration; Near-net-shape; Metal; ceramic composites; Laminated structure

Funding

  1. National Natural Science Foundation of China
  2. Innovation and Entre-preneurship Training Program for Students in Jilin University
  3. [52071155]
  4. [S202210183223]

Ask authors/readers for more resources

We developed a novel method using a combination of direct ink writing and magnet-assisted pressure infiltration to fabricate near-net-shape laminated Al/Al2O3 composites. The effects of sintering temperature and metal layer thickness on the microstructure and mechanical properties of the composites were investigated. It was found that an increase in sintering temperature and a decrease in metal layer thickness led to an increase in bending strength but a decrease in crack-growth toughness of the composites. The fracture behavior of the composites depended on the structural orientation, with cracks initiated in either the metal or ceramic layer depending on the loading direction.
We developed a novel approach involving a combination of direct ink writing and magnet-assisted pressure infiltration to the fabrication of near-net-shape laminated Al/Al2O3 composites. Furthermore, we investigated the effects of the sintering temperature and metal layer thickness on the microstructure and mechanical properties of the resultant composites. With an increase in the sintering temperature and a decrease in the metal layer thickness, the composite's bending strength increased, but its crack-growth toughness decreased. Notably, the fracture behavior of the composite depended on the structural orientation. When the loading direction was parallel to the ceramic lamellae, a crack was initiated in the metal layer since the Al layer was weaker than the ceramic layer. By contrast, a crack was initiated in the ceramic layer when the loading direction was perpen-dicular to the ceramic lamellae. The toughening mechanisms mainly included plastic deformation of the metal matrix, crack deflection, and ligament bridging.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available