Synthesis and hydrolytic degradation of poly (glycerol succinate) based polyesters

Journal

JOURNAL OF THE INDIAN CHEMICAL SOCIETY
Volume 100, Issue 1, Pages -

Publisher

ELSEVIER
DOI: 10.1016/j.jics.2022.100841

Keywords

Polyester; Glycerol; Esterification; Catalyst; Synthesis; Hydrolysis

Ask authors/readers for more resources

This study synthesized glycerol and succinic acid-based polyesters and characterized them using various techniques. The addition of different dicarboxylic acids increased the thermal stability of poly (glycerol succinate). The hydrolytic degradation of polyesters was found to be influenced by the pH of the medium, with significant degradation occurring under basic conditions.
The limited availability of petroleum resources motivates the research towards value-added products production from bio-resources. This study reports the synthesis of glycerol and succinic acid-based polyesters and their detailed characterization. The modification of poly (glycerol succinate) was done by using other diacids like glutaric acid, adipic acid, azelaic acid, sebacic acid, and dodecanedioic acid. The sysnthesized polyesters were characterized using various techniques such as thermogravimetric analysis (TGA), Fourier-transform infrared spectroscopy (FTIR), Nuclear magnetic resonance (NMR), differential scanning calorimetry (DSC), and scanning electron microscopy (SEM). The addition of different dicarboxylic acids to poly (glycerol succinate) based copolyesters increased the thermal stability of poly (Glycerol succinate). Glass transition temperatures were obtained in the range of -17.2 to -22.5 C and it increased with chain length. The progress of reaction was monitored by determining acid number, ester number, and degree of esterification. The hydrolytic degradation of polyesters was carried out in acidic and basic medium. The polyesters was found to degrade under basic conditions whereas no weight loss of poly (glycerol succinate) was found under acidic conditions. Particularly, about 40% of poly (glycerol succinate) was degraded within 24 h under basic conditions (pH = 12). The analysis of morphology of polyesters during degradation showed that the increase in hydrolysis time increased the heterogeneity in polyester matrix.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.0
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available