Eco-friendly recovery of base and precious metals from waste printed circuit boards by step-wise glycine leaching: Process optimization, kinetics modeling, and comparative life cycle assessment

Journal

JOURNAL OF CLEANER PRODUCTION
Volume 389, Issue -, Pages -

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/j.jclepro.2023.136016

Keywords

WPCB; Glycine; Gold extraction; E-waste; Recycling

Ask authors/readers for more resources

This study aims to investigate the step-wise glycine leaching of base and precious metals from waste printed circuit boards (WPCBs) as a green alternative to cyanide for gold leaching. The optimal conditions for selective copper extraction were found to be 0.5 M glycine, 1% v/v H2O2, 20 g/l pulp density, and ambient temperature, achieving a recovery rate of 99.96%. Gold leaching in the glycine + permanganate system was studied, and it was found that 96.17% of the gold can be selectively extracted at the conditions of 4 g/l glycine, 2 g/l potassium permanganate, and room temperature. Activated carbon can be used to separate about 100% of the gold from the leach solution.
Glycine as a green alternative to cyanide for gold leaching is a promising reagent to put a curb on the envi-ronmental footprints of conventional hydrometallurgical processes. This work was designed to investigate the step-wise glycine leaching of the base and precious metals from waste printed circuit boards (WPCBs) as one of the most dominant and problematic e-wastes in today's world. Using response surface methodology, selective copper extraction reached 99.96% recovery at the optimum condition of 0.5 M glycine, 1% v/v H2O2, 20 g/l pulp density, and ambient temperature. Copper sulfide was then recovered from the leach solution via precipitation by sodium hydrosulfide. Gold leaching in the glycine + permanganate system was thoroughly studied with an emphasis on the process's kinetics mechanisms. It was revealed that gold leaching in the glycine and perman-ganate system starts with a rapid phase followed by a slower chemically controlled phase. At the optimum condition of 4 g/l glycine, 2 g/l potassium permanganate, and room temperature, 96.17% of the gold was selectively extracted. By using 3 g/L activated carbon, about 100% of the gold was separated from the leach solution. Comparative life cycle assessment revealed that in the proposed process, the main contributor to most of the environmental impact categories is glycine. Replacing the first step of glycine copper leaching with nitric acid can substantially reduce the environmental footprints of the process to a lower level than many other proposed recycling routes.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available