4.7 Article

Visible-Light Photocatalytic Water Splitting and Norfloxacin Degradation by Reduced Graphene Oxide-Coupled MnON Nanospheres

Journal

ACS APPLIED ENERGY MATERIALS
Volume 5, Issue 10, Pages 12851-12859

Publisher

AMER CHEMICAL SOC
DOI: 10.1021/acsaem.2c02455

Keywords

MnON; HER; OER; photocatalysis; water splitting

Funding

  1. National Research Foundation of Korea
  2. [NRF-2020R1I1A3054429]

Ask authors/readers for more resources

Photocatalytic water splitting using nanocomposites of manganese oxynitride and reduced graphene oxide showed enhanced efficiency due to large surface area, increased light absorption, and interfacial charge transfer. The hydrogen evolution rates increased with the content of graphene oxide in the composites, indicating the important role of reduced graphene oxide. The photocatalysts also displayed stability and recyclability after multiple uses.
Photocatalytic water splitting has gained considerable attention owing to the sustainable nature of hydrogen as a clean energy source alternative to fossil fuels. In this study, nanocomposites consisting of manganese oxynitride and reduced graphene oxide were synthesized by the combined involvement of a solvothermal process and Hummer's method and examined for their photocatalytic applications for water splitting hydrogen production and degradation of norfloxacin as a model pollutant. Spectroscopic and structural analyses showed successful formation of the stable composite in which manganese oxynitride nanoparticles are decorated on graphene sheets. With increasing content of graphene oxide in the composite, it showed the enhanced photocatalytic efficiency in water splitting hydrogen evolution. This is well explained by the large surface area, more light absorption, and interfacial charge transfer in the composite photocatalyst. The hydrogen evolution rates of MnON nanoparticles and MnON/RGO composites of mass ratios 1:1, 1:2, and 1:3 were measured as 250.1, 456.2, 543.6, and 708.5 mu mol g-1 min-1, respectively, and the oxygen evolution rates were measured as 129.0, 229.4, 273.4, and 354.6 mu mol g-1 min-1, respectively, suggesting the important roles of reduced graphene oxide. The photocatalysts also demonstrated enhanced stability and recyclability after multiple uses.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available