Carbon-Binder Weight Loading Optimization for Improved Lithium-Ion Battery Rate Capability

Journal

JOURNAL OF THE ELECTROCHEMICAL SOCIETY
Volume 169, Issue 7, Pages -

Publisher

ELECTROCHEMICAL SOC INC
DOI: 10.1149/1945-7111/ac7ef9

Keywords

-

Funding

  1. U.S. DOE Office of Vehicle Technology Energy Storage Program, eXtreme Fast Charge and Cell Evaluation of Lithium-Ion Batteries (XCEL) Program
  2. National Renewable Energy Laboratory, United States
  3. U.S. Department of Energy (DOE) [DE-AC36-08GO28308]
  4. U.S. Department of Energy Office of Science Laboratory [DE-AC02-06CH11357]
  5. U.S. Department of Energy [DE-AC07-05ID14517]

Ask authors/readers for more resources

Battery performance is influenced by electrode microstructure and weight loading of electrode components. Optimal additive loading can enhance ionic transport and improve battery performance, especially for fast charging.
Battery performance is strongly correlated with electrode microstructure and weight loading of the electrode components. Among them are the carbon-black and binder additives that enhance effective conductivity and provide mechanical integrity. However, these both reduce effective ionic transport in the electrolyte phase and reduce energy density. Therefore, an optimal additive loading is required to maximize performance, especially for fast charging where ionic transport is essential. Such optimization analysis is however challenging due to the nanoscale imaging limitations that prevent characterizing this additive phase and thus quantifying its impact on performance. Herein, an additive-phase generation algorithm has been developed to remedy this limitation and identify percolation threshold used to define a minimal additive loading. Improved ionic transport coefficients from reducing additive loading has been then quantified through homogenization calculation, macroscale model fitting, and experimental symmetric cell measurement, with good agreement between the methods. Rate capability test demonstrates capacity improvement at fast charge at the beginning of life, from 37% to 55%, respectively for high and low additive loading during 6C CC charging, in agreement with macroscale model, and attributed to a combination of lower cathode impedance, reduced electrode tortuosity and cathode thickness.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.6
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available