4.7 Article

Bond behavior between GFRP bars and seawater sea-sand fiber-reinforced ultra-high strength concrete

Journal

ENGINEERING STRUCTURES
Volume 254, Issue -, Pages -

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/j.engstruct.2021.113787

Keywords

Glass fiber-reinforced polymer (GFRP) bars; Ultra-high strength concrete; Seawater sea-sand concrete; Bond strength; Polyethylene (PE) fibers; Pull-out test; Design code assessment

Funding

  1. Natural Science Foundation of China [52008116, 12032009]
  2. Guangzhou Science and Technology Department [201904010163]
  3. Natural Science Foundation of Guangdong Province [2019A1515011637, 2021B1515020029]
  4. Guangzhou Education Bureau [202032852]

Ask authors/readers for more resources

This study investigates the bond characteristics of glass fiber reinforced polymer (GFRP) bars in fiber reinforced ultra-high strength SSC through a series of pull-out tests. The results show that larger bar diameter and longer anchorage length lead to bond strength reductions, and adding 0.5% PE fiber in SSC increases the bond strength.
To tackle the challenge of steel corrosion in conventional reinforced concrete (RC) structures, particularly in maritime environment, the implementation of glass fiber reinforced polymer (GFRP) bars in seawater sea-sand concrete (SSC) structures becomes increasingly popular due to their excellence corrosion resistance. However, the bond characteristics of GFRP bars in fiber reinforced ultra-high strength SSC have not been explored. To this end, a series of pull-out tests on 63 specimens were performed in this study to investigate the influences of different GFRP bar diameters of (i.e., 6 mm, 10 mm and 16 mm), anchorage lengths (i.e., 2.5 and 5 times of the bar diameter), concrete types (SSC and conventional concrete), and polyethylene (PE) fiber contents (i.e., 0, 0.5% and 1% volume fraction) on bond characteristics. The results show that similar to FRP-conventional concrete bond joints, larger bar diameter and longer anchorage length would lead to bond strength reductions for FRP-SSC bond joints. A 0.5% PE fiber addition in SSC would lead to a 3-10% increase in bond strength. However, further increase in PE content to 1% may not necessarily result in further increase in bond strength. Furthermore, the assessment of different design codes revealed that, although ACI440.1R-15 yielded relatively more accurate estimations for bond strength than other design codes, the bond strength could be overestimated if the bar diameter is greater than 16 mm or the anchorage length is less than 5 times the bar diameter.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available