Behaviors of impurity elements Ca and Fe in vanadium-bearing stone coal during roasting and its control measure

Journal

INTERNATIONAL JOURNAL OF MINERAL PROCESSING
Volume 148, Issue -, Pages 100-104

Publisher

ELSEVIER SCIENCE BV
DOI: 10.1016/j.minpro.2016.01.013

Keywords

Roasting; Calcium Iron; Stone coal; Reducing impurities

Funding

  1. Natural Science Foundation of Hubei Province of China [2015CFB221]
  2. Fundamental Research Funds for the Central Universities (WUT) [2015IVA030]
  3. Ministry of Science and Technology of China [2011BAB05B01]

Ask authors/readers for more resources

The behaviors of impurity elements Ca and Fe in vanadium-bearing stone coal during roasting were investigated in two aspects: combining with vanadium and reacting with other phases. As compared to Na, Ca was more easily combined with vanadium generating water-insoluble calcium-bearing vanadate during roasting. The phase distribution calculated by FactSage showed that Ca reacted with quartz and albite to form amorphous phases, resulting in the entrapment of vanadium, thereby decreasing vanadium recovery markedly. In contrast, Fe in stone coal did not affect vanadium recovery as it did not combine with vanadium and not react with other phases during roasting. In order to decrease the negative effects derived from the impurity elements such as Ca, a control measure of concentrating vanadium and reducing impurities treatment was carried out to decrease the dosage of Na2SO4 and improve vanadium recovery. (C) 2016 Elsevier B.V. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.1
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available