4.7 Article

Block Copolymer and Nanosilica-Modified Epoxy Nanocomposites

Journal

ACS APPLIED POLYMER MATERIALS
Volume 3, Issue 8, Pages 4156-4167

Publisher

AMER CHEMICAL SOC
DOI: 10.1021/acsapm.1c00619

Keywords

block copolymers; silica; epoxy; fracture toughness; dispersion; compact tension

Funding

  1. 3M Company
  2. 3M Science and Technology Fellowship
  3. NSF through the MRSEC program
  4. Northwestern University
  5. Dow Chemical Company
  6. DuPont de Nemours, Inc.
  7. State of Illinois through the Department of Commerce
  8. Board of Education (HECA)
  9. U.S. Department of Energy Office of Energy Research
  10. U.S. National Science Foundation (NSF) Division of Materials Research

Ask authors/readers for more resources

The study evaluated the effects of nanoscale silica particle additives on the tensile properties of modified epoxies, showing an increase in modulus and toughness. Combining BCP and nanosilica additives resulted in a synergistic effect, enhancing the toughness of the epoxy beyond that obtained with individually modified formulations.
The effects of nanoscale silica particle additives on the tensile properties of neat and poly(ethylene-alt-propylene)-b-poly(ethylene oxide) block copolymer (BCP)-modified epoxies were evaluated. Nanosilica and BCP modifiers were dispersed both individually and together in epoxy formulations. The nanosilica formed a stable dispersion, and BCP modifiers formed well-dispersed spherical micelle nanostructures in the matrix. When both additives were used, BCP micelles were observed to adsorb on nanosilica surfaces, resulting in limited aggregation of nanosilica particles. Tensile tests on bulk specimens showed that the addition of nanosilica to both neat and BCP-modified epoxy formulations increased the modulus of the composites. Compact tension tests also revealed increases in the critical stress intensity factor, K-Ic, and critical strain energy release rate, G(Ic), in both the block copolymer and nanosilica-modified epoxies. Combining both additives in the epoxy enhanced toughness beyond that obtained with the individually modified formulations. Increasing nanosilica loading up to 25 wt % produced a monotonic increase in the modulus and G(Ic). The nanocomposite with 25 wt % nanosilica reached an optimal level of toughness at low BCP concentrations (ca. 4 wt %). Scanning electron micrographs obtained from fracture surfaces revealed topological features indicative of micelle cavitation and nanosilica debonding, toughening mechanisms that operate in concert.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available