The study found that the presence of crumb rubber (CR) in asphalt binder can increase viscosity and improve rutting resistance, but is detrimental to cracking properties.
The crumb rubber modified (CRM) binder was evaluated considering the general operating temperatures of high, intermediate, and low temperatures. CRM binders were produced with four different contents (0, 5, 10, and 15%) using the base asphalt binder (PG64-22). Then, they were artificially aged by a rolling thin-film oven (RTFO) and pressure aging vessel (PAV). Superpave binder tests using a rotational viscometer (RV), dynamic shear rheometer (DSR), and bending beam rheometer (BBR) was applied to characterize the performance of the original and aged binders. Multiple stress creep recovery (MSCR) tests were also performed for deeper rutting characterization. The results of this study are as follows: (1) the presence of PR increases the binder viscosity, (2) the integration of CRM greatly improved the rutting resistance of the binder, and it was found that PR also improved the rutting characteristics, and (3) it is observed that PR is detrimental to the cracking properties of CRM binders.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.6
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available