Copper-doped zinc oxide (ZnO:Cu) thin films were deposited on glass substrates using ultrasonic spray pyrolysis technique, and the effect of water content on methylene blue (MB) dye degradation through a photocatalytic process was studied. Different films exhibited varying degradation behaviors, with the photocatalytic response related to the surface morphology. Films deposited with 80% water content showed more promising MB degradation for UV exposure times longer than 180 min.
Copper-doped zinc oxide (ZnO:Cu) thin films were deposited by an ultrasonic spray pyrolysis technique on glass substrates. Doping concentration was maintained at 3 at %, and the deposition temperature was 450 degrees C. The water content in the starting solution was varied in order to study its effect on the degradation of methylene blue (MB) dye by a photocatalytic process. X-ray diffraction patterns confirm the ZnO wurtzite structure and scanning electron microscopy analysis shows morphologies with different types of grains with average sizes varying from 90 to 300 nm. All the films achieved a maximum MB degradation of about 74% for a UV light exposition time of 180 min. However, the degradation behavior with respect to UV exposition time is different for each film. Two different degradation rates (0-90 min and 120-180 min exposure times, respectively) were performed for all ZnO films, and their photocatalytic response is related to the obtained surface morphology, which is explicated in this work. The films deposited with 80% water content in the starting solution are more promising for MB degradation when the UV exposure times are longer than 180 min.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.5
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available