Enhanced crystallization and storage stability of mechanical properties of biosynthesized poly (3-hydroxybutyrate-co-3-hydroxyhexanate) induced by self-nucleation

Journal

INTERNATIONAL JOURNAL OF BIOLOGICAL MACROMOLECULES
Volume 184, Issue -, Pages 797-803

Publisher

ELSEVIER
DOI: 10.1016/j.ijbiomac.2021.06.120

Keywords

Self-nucleation; Crystallization; Poly(3-hydroxy burate co-3 hydrodocyhexanate)

Funding

  1. Natural Science Foundation of Jiangsu Province [BK20200606]
  2. China Postdoctoral Science Foundation [2021M691267]
  3. National Natural Science Foundation of China [51873082, 52073123]
  4. Fundamental Research Funds for the Central Universities [JUSRP121034]
  5. Opening Project of Beijing Key Laboratory of Quality Evaluation Technology for Hygiene and Safety of Plastics (Beijing Technology and Business University) [QETHSP2020012]

Ask authors/readers for more resources

By utilizing high melting point poly (3-hydroxybutyrate) as a nucleating agent and controlling the processing temperature and PHB content, the crystallization rate and crystal nucleus density of PHBH can be significantly increased, while secondary crystallization is inhibited, improving its mechanical performance and storage stability.
The poor mechanical properties induced by unsatisfactory crystallization ability limit the widespread use of biosynthesized poly (3-hydroxybutyrate-co-3-hydroxyhexanate) (PHBH). In this work, poly (3-hydroxybutyrate) (PHB) with a high melting point was first used as a homogeneous nucleating agent to increase the crystallization rate of PHBH by a self-nucleation method with a wider processing temperature window and crystallization kinetics and storage stability of mechanical properties of the PHBH/PHB mixtures were systematically investigated. By controlling the processing temperature and PHB content, the crystal nucleus density and crystallization rate of PHBH could be greatly increased while secondary crystallization was inhibited. When the processing temperature is 185 degrees C and PHB content is 20 wt%, the half crystallization time is shortened by 96% and the crystallinity was increased to 37.2%. Meanwhile, the mechanical performance of PHBH and its storage stability are greatly improved. Therefore, this work provides a simple and efficient way to improve the crystallization and mechanical performance of PHBH, which is expected to be applied to industrial production on a large scale.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available