Influence of the synthetic calcium aluminate hydrate and the mixture of calcium aluminate and silicate hydrates on the compressive strengths and the microstructure of metakaolin-based geopolymer cements*

Journal

MATERIALS CHEMISTRY AND PHYSICS
Volume 264, Issue -, Pages -

Publisher

ELSEVIER SCIENCE SA
DOI: 10.1016/j.matchemphys.2021.124459

Keywords

Bauxite; Eggshell; Calcium aluminate hydrate; Rice husk ash; Metakaolin; Geopolymer cements

Funding

  1. Alexander von Humboldt-Stiftung [KAM/1155741 GFHERMES-P]

Ask authors/readers for more resources

The study found that adding 10 wt% of CA04 and 20 wt% of (CA04 + CS04) can significantly increase the compressive strength of geopolymer cements and decrease the pore size, leading to improved strength development.
The main goal of this study is to investigate the effects of the calcium aluminate hydrate (CA04) and the mixture of calcium aluminate and silicate hydrates (CA04 + CS04) on the compressive strengths and the microstructure of metakaolin-based geopolymer cements. Bauxite, rice husk and eggshells were calcined and mixed in proper amounts to prepare CA04 and CS04. Metakaolin has been substituted by 0, 5, 10, 15 and 20 wt% of CA04, 10 and 20 wt% of (CA04 + CS04) in the formulation of geopolymer cements. The clay-like solid materials were characterized by measuring their compressive strengths, the crystalline and amorphous phases were monitored using the X-ray diffractometry analysis, their microstructures were investigated using the scanning electron microscope and mercury intrusion porosimetry and the functional groups were studied using the infrared spectroscopy. The compressive strengths of geopolymer cements containing 0, 5, 10, 15 and 20 wt% of CA04 are 49.50, 57.17, 63.59, 38.79 and 35.05 MPa, respectively. Those containing 10 and 20 wt% of (CA04 + CS04) are 40.59 and 51.19 MPa, respectively. The average pore diameters of geopolymer cements containing 0, 10 and 20 wt% of CA04 are 11.80, 10.10, 12.20 nm, respectively. Whereas the one containing 20 wt% of (CA04 + CS04) is 10.80 nm. It appears that geopolymer cement with 10 wt% of CA04 and 20 wt% of (CA04 + CS04) have higher compressive strengths and lower average pore diameters. It was found that 10 and 20 wt% of CA04 and (CA04 + CS04), respectively, could be used as additives for the preparation of geopolymer cements with higher strength development.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.6
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available