4.8 Article

High-performance half-Heusler thermoelectric devices through direct bonding technique

Journal

JOURNAL OF POWER SOURCES
Volume 493, Issue -, Pages -

Publisher

ELSEVIER
DOI: 10.1016/j.jpowsour.2021.229695

Keywords

Waste heat recovery; Thermoelectric; Half-Heusler; Contact resistance; Efficiency; Air stability; Direct bonding; Metallization

Funding

  1. DARPA MATRIX program (NETS)
  2. NSF-CREST [HRD 1547771]
  3. Office of Naval Research [N00014-20-1-2602]
  4. Army RIF program
  5. National Science Foundation IUCRC: Center for Energy Harvesting Materials and Systems

Ask authors/readers for more resources

This study demonstrates a TEG fabrication process that can achieve high electrical conversion efficiency at high temperatures by reducing thermal and electrical resistances between metal electrodes and TE legs, improving TEG performance and stability.
Solid-state thermoelectric generators (TEGs) are promising solution for waste heat recovery. However, they typically suffer from lower conversion efficiency, lack of reliable high temperature device fabrication process and long-term stability. In order to realize high electrical conversion efficiency (ECE) in TEGs, it is critical that in conjunction with high TE materials figure of merit, zT, there is also a reliable TE module fabrication process. This study demonstrates the TEG fabrication process that results in reduced thermal and electrical contact resistances between metal electrodes and TE legs, even at high temperatures (>600 ?C). The fabrication approach is demonstrated using p-type ZrCoSb-based and n-type ZrNiSn-based half-Heusler TE materials. High temperature brazing material is used as a filler that enables direct bonding of TE legs to the copper electrode without metallizing legs. This technique improves the TEG performance and stability at high temperatures by minimizing the contact resistance and diffusion at TE leg/electrode interface. The fabricated modules exhibit a high power density of -11.5 Wcm? 2 and an ECE of 9.5% at 670 ?C temperature gradient. The module was exposed to longtime soaking at 550 ?C in air and was found to exhibit negligible deterioration. These results are highly promising for advancing the TE modules in waste heat recovery applications.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.8
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available