SnS and SnO nanocomposites with different x values (0, 3.57%, 7.16%, and 10.79%) have been successfully synthesized, showing a positive Seebeck coefficient for p-type conduction. The ZT value increases with increasing x, with a 55% enhancement compared to pure SnS at 325K.
(SnS)(1-x)(SnO)(x) : x = 0, 3.57%, 7.16%, and 10.79% nanocomposites (NCs) have been successfully synthesized using a simple polyol method. XRD data analysis shows formation of SnS and SnO NCs with an average crystallite size in the range from 30 to 35 nm. The Rietveld refinement analysis indicates layered orthorhombic crystal structure. FESEM images display the morphology of nanoflakes and nanoplates. Their positive Seebeck coefficients (alpha) suggest the p-type conduction. This is consistent with the deficiency of Sn found. (SnS)(0.9284)(SnO)(0.0716) NC exhibits a thermal conductivity (kappa) of 0.75 Wm(-1) K-1 at 300 K. Electrical (sigma) and thermal conductivities are decreased, but alpha enhances with increasing x. Consequently, the dimensionless figure of merit (ZT) increases with increasing x up to 7.16% for which ZT at 325 K is 0.0036. This is 55% enhancement compared to the pure SnS that opens a new window for improvement of thermoelectric performance near room temperature.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.6
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available