4.7 Article

Comparing the roles of Sb and Bi on microstructures and application properties of the Al-15% Si alloy

Journal

JOURNAL OF ALLOYS AND COMPOUNDS
Volume 878, Issue -, Pages -

Publisher

ELSEVIER SCIENCE SA
DOI: 10.1016/j.jallcom.2021.160343

Keywords

Al-Si; Solidification; Si morphology; Tensile properties; Wear

Funding

  1. FAPESPSAo Paulo Research Foundation, Brazil [2019/236737]
  2. CAPESCoordenacAo de Aperfeicoamento de Pessoal de Nivel Superior, Brazil [001]
  3. CNPqNational Council for Scientific and Technological Development, Brazil

Ask authors/readers for more resources

This study investigates the effects of adding bismuth and antimony to hypereutectic Al-Si alloys through experiments and various analytical methods. The results show that antimony enhances wear resistance and Si growth form, while bismuth improves tensile properties.
The roles of Bismuth (Bi) and Antimony (Sb) additions to hypereutectic Al-Si alloys with significant variation in solidification cooling rates have yet to be unraveled. Both elements are considered of importance in the production chain of Al-based metallurgical products: while Sb is a refiner of the eutectic Si, Bi remains important in applications requiring better levels of alloy machinability. Based on these verified realities, the present research aims to modify the Al-15 wt% Si hypereutectic alloy with 1.0 wt% Bi as well as with 1.0 wt% Sb. The implications of these incorporations on the characteristics of the microstructure phases and the tensile/wear properties are examined. Various samples characterized by distinct solidification rates have been generated through transient directional solidification experiments. Several methods were used to examine and compare the two alloys with each other: microstructure and segregation are investigated by CALPHAD simulations, optical microscopy, scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy (EDS), whereas wear and tensile properties have been determined through standardized measurements. While adding Sb provides the growth of broken Si in the form of lamellae and some fraction of fibers for higher solidification rates, Bi alloying preserves lamellar growth for all rates examined. Adding Bi is better than Sb in reaching higher tensile properties, but Sb presence provides greater wear resistance. Both alloying elements ductilize the brittle Al-15 wt% Si alloy. (c) 2021 Elsevier B.V. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available