4.7 Article

Comparative Assessment of Pretreatment Options for Biomass Pyrolysis: Linking Biomass Compositions to Resulting Pyrolysis Behaviors, Kinetics, and Product Yields

Journal

ENERGY & FUELS
Volume 35, Issue 4, Pages 3186-3196

Publisher

AMER CHEMICAL SOC
DOI: 10.1021/acs.energyfuels.0c04186

Keywords

-

Funding

  1. National Natural Science Foundation of China [51776209, 51876208, 51661145011]
  2. National Key R&D Program of China [2017YFE0124200]
  3. Science and Technology Planning Project of Guangdong Province [2017A020216009, 2015A020215024]
  4. Youth Innovation Promotion Association, CAS [2018383]
  5. Pearl River S&T Nova Program of Guangzhou [201806010061, 201906010092]
  6. Foundation of Key Laboratory of Biofuels, Qingdao Institute of Bioenergy and Bioprocess Technology, Chinese Academy of Sciences [CASKLB201809]

Ask authors/readers for more resources

Four representative pretreatment methods were used to alter eucalyptus compositions and study their effects on pyrolysis behaviors, kinetics, and product yields. All four pretreatment methods significantly decreased the AAEM contents of eucalyptus, with DH and MOP removing hemicellulose or lignin fractions. The activation energy for hemicellulose pyrolysis was reduced by WW, AW, and DH, while all four methods improved cellulose pyrolysis activation energy. Additionally, the formation of certain pyrolysis products was suppressed, and the levoglucosan yield was increased by all four pretreatment methods.
Four representative pretreatment methods, water washing (WW), acid washing (AW), dilute acid hydrolysis (DH), and microwave assisted organosolv pretreatment (MOP), were adopted to alter eucalyptus compositions. The linkages between eucalyptus compositions and the resulting pyrolysis behaviors, kinetics, and product yields were investigated. The results showed that all four pretreatment methods evidently lowered the alkali and alkaline earth metal (AAEM) contents of eucalyptus, while DH and MOP significantly removed hemicellulose or lignin fractions. WW, AW, and DH reduced the activation energy for hemicellulose pyrolysis from 67.88 to 40.41-64.08 kJ/mol, whereas all four pretreatment methods improved that for cellulose pyrolysis from 71.83 to 77.08-205.47 kJ/mol. All four pretreatment methods effectively suppressed the formation of pyrolytic char, H2O, CO, CH4, aldehydes, ketones, and carboxylic acids, while evidently improving the levoglucosan yield. The maximum levoglucosan yield of 49.9% was obtained from eucalyptus pretreated by MOP. The levoglucosan yield was inhibited by the catalytic effects of AAEMs and the interactions between biomass major components.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available