Preparation of Li7P3S11 glass-ceramic electrolyte by dissolution-evaporation method for all-solid-state lithium ion batteries

Journal

ELECTROCHIMICA ACTA
Volume 219, Issue -, Pages 235-240

Publisher

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.electacta.2016.09.155

Keywords

Li7P3S11 glass-ceramic; Solid state electrolyte; Lithium ion battery; Ion conductivity

Funding

  1. program for Innovative Research Team in University of Ministry of Education of China [IRT13037]

Ask authors/readers for more resources

Design/fabrication of solid state electrolytes with high ionic conductivity is of great importance to develop next-generation Li ion batteries. In this work, the Li7P3S11 glass-ceramic electrolyte is successfully synthesized by dissolution-evaporation approach. The solvent effect on the electrochemical performance of Li7P3S11 is investigated by electrochemical impedance spectroscopy and chronoamperometry tests. The Li7P3S11 electrolyte prepared by a solution of acetonitrile has a high ionic conductivity of 9.7 x 10(-4) S cm(-1) at 298 K and a low activation energy of 31.2 kJ mol-(1). Impressively, a wide and stable electrochemical window up to 5 V (vs. Li/Li+) is demonstrated between the solid electrolyte and lithium electrode. The developed dissolution-evaporation approach shows good industrial prospect due to its advantages of energy conservation and high efficiency. (C) 2016 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.6
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available