Nanowire-toughened transition layer to improve the oxidation resistance of SiC-MoSi2-ZrB2 coating for C/C composites

Journal

CORROSION SCIENCE
Volume 111, Issue -, Pages 259-266

Publisher

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.corsci.2016.05.013

Keywords

Ceramic matrix composites; Weight loss; High temperature corrosion

Funding

  1. National Natural Science Foundation of China [51221001, 51572223, 51222207]
  2. Research Fund of State Key Laboratory of Solidification Processing (NWPU), China [12-BZ-2014]
  3. 111 Project [B08040]

Ask authors/readers for more resources

To enhance the oxidation resistance of SiC-MoSi2-ZrB2 coating for C/C composites, pre-oxidation treatment and chemical vapor deposition were applied to construct a SiC nanowire-toughened inlaid transition layer between C/C and SiC-MoSi2-ZrB2 coating. The results show that the coating prepared with pre-oxidation and SiC nanowires has better oxidation resistance, which can protect C/C for 124 h at 1773 K in air with the weight loss per unit area of 1.1 mg cm(-2). The synergistic effect of the inlaid structure of the transition layer and SiC nanowires plays positive role on alleviating the mismatch of thermal expansion coefficient between C/C and SiC-MoSi2-ZrB2 coating. (C) 2016 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available